00596 STRESS CORROSION CRACKING OF STAINLESS ALLOYS IN OXYGENATED CAUSTIC ENVIRONMENTS

Product Number: 51300-00596-SG
ISBN: 00596 2000 CP
Author: Stephen Clarke
$0.00
$20.00
$20.00
The temperatures required to produce fully oxidized white liquor are capable of causing stress corrosion cracking (SCC) on the 300 series of austenitic stainless steels (304L/316L). This report outlines the likely mechanisms for SCC of 316L/304L in white liquor oxidizer systems, and suggests ways in which SCC can be prevented. Case histories are given and alternative alloys are suggested. Keywords: stainless steels, kraft process, stress corrosion cracking, caustic, oxygen, corrosion, nickel-base alloys.
The temperatures required to produce fully oxidized white liquor are capable of causing stress corrosion cracking (SCC) on the 300 series of austenitic stainless steels (304L/316L). This report outlines the likely mechanisms for SCC of 316L/304L in white liquor oxidizer systems, and suggests ways in which SCC can be prevented. Case histories are given and alternative alloys are suggested. Keywords: stainless steels, kraft process, stress corrosion cracking, caustic, oxygen, corrosion, nickel-base alloys.
PRICE BREAKS - The more you buy, the more you save
Quantity
1+
5+
Price
$20.00
$20.00
Product tags
Also Purchased
Picture for 06501 INDUSTRIAL EXPERIENCE ON THE CAUSTIC
Available for download

06501 INDUSTRIAL EXPERIENCE ON THE CAUSTIC CRACKING OF STAINLESS STEELS AND NICKEL ALLOYS - A REVIEW

Product Number: 51300-06501-SG
ISBN: 06501 2006 CP
Author: Raul B. Rebak
$20.00
Picture for 00152 CORROSION PERFORMANCE OF 13CR STAINLESS
Available for download

00152 CORROSION PERFORMANCE OF 13CR STAINLESS STEELS

Product Number: 51300-00152-SG
ISBN: 00152 2000 CP
Author: Trond Rogne, John M. Drugli, Ole Oystein Knudsen, Stein Olsen and Jakob Enerhaug
$20.00