09296 Fracture Analysis of Slow Strain Rate Test for Stress Corrosion Cracking

Recently Crack Growth Rate and Threshold Stress Intentisity Factor  analyses of data from Slow Strain Rate tests have been used for Stress COrrosion Cracking evaluation. This methodology has been discussed in detail based on different analytical techniques and the results from laboratory tests have also been presented.

Product Number: 51300-09296-SG
ISBN: 09296 2009 CP
Author: Russell D. Kane and Anand Venkatesh
Publication Date: 2009
$0.00
$20.00
$20.00

Slow-Strain-Rate (SSR) tests are usually limited to comparative evaluations of Stress Corrosion Cracking (SCC) based on relative changes in ductility parameters such as elongation and reduction in area. Recently Crack Growth Rate (CGR) and Threshold Stress Intentisity Factor (KISCC) analyses of data from SSR tests have been used for SCC evaluation. Benefits of this approach are that the results can be used to develop a detailed engineering analysis. This methodology has been discussed in detail based on different analytical techniques and the results from laboratory tests have also been presented.

Keywords: slow-strain-rate, stress intensity factor, crack growth rate, ethanol

Slow-Strain-Rate (SSR) tests are usually limited to comparative evaluations of Stress Corrosion Cracking (SCC) based on relative changes in ductility parameters such as elongation and reduction in area. Recently Crack Growth Rate (CGR) and Threshold Stress Intentisity Factor (KISCC) analyses of data from SSR tests have been used for SCC evaluation. Benefits of this approach are that the results can be used to develop a detailed engineering analysis. This methodology has been discussed in detail based on different analytical techniques and the results from laboratory tests have also been presented.

Keywords: slow-strain-rate, stress intensity factor, crack growth rate, ethanol

Also Purchased
Picture for 97048 RAPID SCREENING OF STAINLESS STEELS FOR
Available for download

97048 RAPID SCREENING OF STAINLESS STEELS FOR ENVIRONMENTALLY ASSISTED CRACKING IN H2S/CO2/Cl- ENVIRONMENTS USING THE SLOW STRAIN RATE TEST

Product Number: 51300-97048-SG
ISBN: 97048 1997 CP
Author: C.J.B.M. Joia, A.L.L.T. Small, J.A.C. Ponciano, R.D. Kane
$20.00
Picture for 98140 SCC MAPS FOR LOW-ALLOY STEELS BY
Available for download

98140 SCC MAPS FOR LOW-ALLOY STEELS BY SSRT METHOD

Product Number: 51300-98140-SG
ISBN: 98140 1998 CP
Author: Taku Arai, Masami Mayuzumi, Joji Ohta
$20.00
Picture for Use of NACE TM0111 Slow Strain Rate Test for Evaluation of Ethanol SCC
Available for download

Use of NACE TM0111 Slow Strain Rate Test for Evaluation of Ethanol SCC

Product Number: 51315-5945-SG
ISBN: 5945 2015 CP
Author: Russell Kane
Publication Date: 2015
$20.00