51318-11201-EFFECT OF ANNEALING TEMPERATURE ON PITTING CORROSION BEHAVIOR OF A LEAN DUPLEX STAINLESS STEEL
-
Home
/
-
Conference Papers
/
-
51318-11201-EFFECT OF ANNEALING TEMPERATURE ON PITTING CORROSION BEHAVIOR OF A LEAN DUPLEX STAINLESS STEEL
Also Purchased
Available for download
Product Number:
51318-11200-SG
Author:
Heike Hattendorf / Jutta Kloewer / Alejandra López
Publication Date:
2018
$20.00
We're sorry, something went wrong.
We are unable to complete this action. Please try again at a later time.
If this error continues to occur, please contact NACE First Service for assistance.
Use this error code for reference:
Please login to use NACE Standards Credits*
* NACE Members receive NACE Standards Credits in order to redeem eligible NACE Standards and Reports in the Store
You are not a NACE Member.
NACE Members enjoy many benefits, including NACE Standards Credits which can be used to redeem eligible NACE Standards and Reports in the Store.
You can visit the NACE Membership Page to learn about the benifits of NACE membership.
You have previously purchased this item.
Go to Downloadable Products in your NACE Store profile to find this item.
You do not have sufficient NACE Standards Credits to claim this item.
Click on 'ADD TO CART' to purchase this item.
Your NACE Standards Credit(s)
Please review your transaction.
Click on 'REDEEM' to use your NACE Standards Credits to claim this item.
Your NACE Standards Credit(s)
You have successfully redeemed:
Go to Downloadable Products in your NACE Store Profile to find and download this item.
Available for download
Product Number:
51318-11218-SG
Author:
Hanan Farhat
Publication Date:
2018
$20.00
We're sorry, something went wrong.
We are unable to complete this action. Please try again at a later time.
If this error continues to occur, please contact NACE First Service for assistance.
Use this error code for reference:
Please login to use NACE Standards Credits*
* NACE Members receive NACE Standards Credits in order to redeem eligible NACE Standards and Reports in the Store
You are not a NACE Member.
NACE Members enjoy many benefits, including NACE Standards Credits which can be used to redeem eligible NACE Standards and Reports in the Store.
You can visit the NACE Membership Page to learn about the benifits of NACE membership.
You have previously purchased this item.
Go to Downloadable Products in your NACE Store profile to find this item.
You do not have sufficient NACE Standards Credits to claim this item.
Click on 'ADD TO CART' to purchase this item.
Your NACE Standards Credit(s)
Please review your transaction.
Click on 'REDEEM' to use your NACE Standards Credits to claim this item.
Your NACE Standards Credit(s)
You have successfully redeemed:
Go to Downloadable Products in your NACE Store Profile to find and download this item.
Available for download
Product Number:
51318-11212-SG
Author:
William Kovacs III / Liu Cao / Byron Mohr / Nicholas Burkardt / Zachary Berg
Publication Date:
2018
$20.00
We're sorry, something went wrong.
We are unable to complete this action. Please try again at a later time.
If this error continues to occur, please contact NACE First Service for assistance.
Use this error code for reference:
Please login to use NACE Standards Credits*
* NACE Members receive NACE Standards Credits in order to redeem eligible NACE Standards and Reports in the Store
You are not a NACE Member.
NACE Members enjoy many benefits, including NACE Standards Credits which can be used to redeem eligible NACE Standards and Reports in the Store.
You can visit the NACE Membership Page to learn about the benifits of NACE membership.
You have previously purchased this item.
Go to Downloadable Products in your NACE Store profile to find this item.
You do not have sufficient NACE Standards Credits to claim this item.
Click on 'ADD TO CART' to purchase this item.
Your NACE Standards Credit(s)
Please review your transaction.
Click on 'REDEEM' to use your NACE Standards Credits to claim this item.
Your NACE Standards Credit(s)
You have successfully redeemed:
Go to Downloadable Products in your NACE Store Profile to find and download this item.
We're sorry, something went wrong.
We are unable to complete this action. Please try again at a later time.
If this error continues to occur, please contact NACE First Service for assistance.
Use this error code for reference:
Please login to use NACE Standards Credits*
* NACE Members receive NACE Standards Credits in order to redeem eligible NACE Standards and Reports in the Store
You are not a NACE Member.
NACE Members enjoy many benefits, including NACE Standards Credits which can be used to redeem eligible NACE Standards and Reports in the Store.
You can visit the NACE Membership Page to learn about the benifits of NACE membership.
You do not have sufficient NACE Standards Credits to claim this item.
Click on 'ADD TO CART' to purchase this item.
Your NACE Standards Credit(s)
Please review your transaction.
Click on 'REDEEM' to use your NACE Standards Credits to claim this item.
Your NACE Standards Credit(s)